Product Name | Nickel or Nickel Based Alloy Electrode | ||||||||||
Product No. | MHAE411-WE073 | ||||||||||
Standard | |||||||||||
GB | ENiCrFe-1 | ||||||||||
AWS | ENiCrFe-1 | ||||||||||
JIS | DNiCrFe-1 | ||||||||||
Type of electrode | Low hydrogen | ||||||||||
Welding Position | F,V,OH,H | ||||||||||
Chemical Composition | C | Mn | Fe | P | S | Si | Cu | Ni | Cr | Nb+Ta | other |
Guarantee | ≤0.10 | 1.0-3.5 | ≤12.0 | ≤0.03 | ≤0.02 | ≤0.75 | ≤0.50 | ¡Ý62 | 13.0-17.0 | 0.5-2.5 | ≤0.50 |
Mechanical Properties of Deposited Metal | |||||||||||
Test Item | Tensile Strengh Rm (MPa) | Elongation A4 (%) | |||||||||
Guarantee | ¡Ý550 | ¡Ý30 | |||||||||
Reference Current (AC or DC) | |||||||||||
Electrode Diameter(mm) | 2.5 | 3.2 | 4.0 | ||||||||
Welding Current(A) | 40-70 | 80-100 | 110-150 | ||||||||
Instructions | |||||||||||
1.The Electrodes must be baked under 300~350 for an hour before Welding and used as soon as baking is completed. | |||||||||||
2.The stains on the weldments,such as rust,oil stains,moisture,etc.,must be cleared away before Welding. | |||||||||||
Application | |||||||||||
It is suitable for welding NiCrFe alloys (UNS N08800,UNS N06600)and for welding dissimilar metals. |